Chemical etching services for microelectronics

Precision photochemical etching for hermetic lids, leadframes, and EMI shielding. Burr-free, stress-free parts from prototype to volume.

Request a quote

Stepped hermetic window lid
0.004” to 0.060”(0.10 to 1.52 mm) material thickness
±0.004”general tolerance
±0.002”tight tolerance

Materials we etch

Kovar, stainless steel, Invar, Alloy 42, mild steel, and copper in all grades, including oxygen-free.

Components we make

Stepped lids, flat lids, window lids, leadframes, and EMI/RFI shielding.

Why chemical etching

Burr-free edges

No mechanical force, so no burrs to remove.

No added stress

The chemical process doesn’t introduce stresses that change material properties.

No localized heat

Material integrity is preserved without thermal distortion.

Low tooling cost

Well suited to prototypes and high-volume runs alike.

Faster iterations

Design changes don’t require new hard tooling, so turnaround stays short.

The chemical etching process

  1. 1

    Prepare

    Raw material is laminated with a dry film resist.

  2. 2

    Expose

    The design is applied with UV light.

  3. 3

    Develop

    Exposed resist is developed to reveal the metal.

  4. 4

    Etch

    The metal is etched away to form the part.

  5. 5

    Finish

    Parts are tagged in sheet form for easy handling and downstream processing.

Chemical etching process diagram: material preparation, cleaning, resist lamination, UV exposure, developing, etching, and resist removal

Have a part to etch?

Send your drawing, material, and quantities, and we’ll confirm tolerances and lead time.