Over time, epoxies and RF absorbers can outgas organics inside a hermetic package after sealing. This type of contamination can lead to poor device performance and ultimately device failure. The Hi-Rel manufactures several getter solutions that address the outgassing of organics as detailed below.
Hi-Rel and Johnson Matthey have been teaming together since 1999 to bring our customers the most robust solutions. Each solution is customized based on application, footprint, RGA analysis and other factors. We work together early in your design process so that whatever organics contaminant issue your electronics face, we customize your exact solutions.
Let us know how we can help.
| Offering | Form factor | H₂ | H₂O | CO₂ | O₂ | Organics | Activation | Temp max | Absorption rate | Capacity |
|---|
| HR1 Series | Pd metal foil (0.002" / 0.004") | ✓ | — | — | — | — | No | 500°C (operating) | 455 ppm/in²/min (H₂) | 20 cc/cc (H₂) |
| HGI Series | Dispensed/printed on lid/coupon | ✓ | ✓ | ✓ | — | ✓ | 4hrs at 100°C | 120°C (processing) | — | — |
| HTI Series | Dispensed/printed on lid/coupon | ✓ | ✓ | ✓ | — | ✓ | 4hrs at 100°C | 320°C (processing) | — | — |
| HTA Series | Tablet | ✓ | ✓ | ✓ | — | ✓ | Optional (pre-activated) | 400°C (effective) | — | — |
| CP Series | Tablet | ✓ | ✓ | ✓ | — | ✓ | Required (normally) | 500°C (processing/storage) | — | — |
| CP Vacuum Series | Tablet | ✓ | ✓ | ✓ | ✓ | ✓ | Activate during pump down (250°C) | NS | — | — |